陈翔峰,穆振军,许春生,任润桃.铜及铜合金在厦门海域实海暴露腐蚀规律研究[J].装备环境工程,2013,10(2):1-3,24. CHEN Xiang-feng,MU Zhen-jun,XU Chun-sheng,REN Run-tao.Corrosion Rule of Copper and Its Alloys Exposed in Xiamen Natural Seawater[J].Equipment Environmental Engineering,2013,10(2):1-3,24.
铜及铜合金在厦门海域实海暴露腐蚀规律研究
Corrosion Rule of Copper and Its Alloys Exposed in Xiamen Natural Seawater
投稿时间:2012-10-06  修订日期:2013-03-01
DOI:
中文关键词:    铜合金  实海暴露
英文关键词:copper  copper alloy  seawater exposure
基金项目:
作者单位
陈翔峰 海洋腐蚀与防护国防科技重点实验室,福建厦门361101;中船重工七二五研究所厦门分部,福建厦门361101 
穆振军 中船重工七二五研究所厦门分部,福建厦门361101 
许春生 中船重工七二五研究所厦门分部,福建厦门361101 
任润桃 海洋腐蚀与防护国防科技重点实验室,福建厦门361101;中船重工七二五研究所厦门分部,福建厦门361101 
AuthorInstitution
CHEN Xiang-feng State Key Laboratory for Marine Corrosion and Protection,Xiamen361101,China;Xiamen Branch of Luoyang Ship Material Research Institute,Xiamen361101,China 
MU Zhen-jun Xiamen Branch of Luoyang Ship Material Research Institute,Xiamen361101,China 
XU Chun-sheng Xiamen Branch of Luoyang Ship Material Research Institute,Xiamen361101,China 
REN Run-tao State Key Laboratory for Marine Corrosion and Protection,Xiamen361101,China;Xiamen Branch of Luoyang Ship Material Research Institute,Xiamen361101,China 
摘要点击次数:
全文下载次数:
中文摘要:
      通过对TUP纯铜、B10铜合金与B30铜合金3种典型材料在厦门海域进行实海暴露挂片试验,总结了3种材料在厦门海域全浸区、潮差区及飞溅区3个不同区域的腐蚀规律,对其腐蚀机理进行了简要探讨,并对其长周期腐蚀行为作出了预测。
英文摘要:
      In this article, 3kinds of typical copper and its alloys, including Tup pure copper, B10, and B30copper alloys, were exposed in3zones of seawater at Xiamen. The corrosion rules of the three materials in immersion zone, tidal range zone, and splash zone were summarized, and the corrosion mechanism was discussed, and the long-term corrosion character was also predicted.
查看全文  查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第12768167位访问者    渝ICP备15012534号-5

版权所有:《装备环境工程》编辑部 2014 All Rights Reserved

邮编:400039     电话:023-68792835    Email: zbhjgc@163.com

视频号 公众号