周堃,钱翰博,周漪,王成章,王津梅.导弹非金属薄弱环节贮存寿命快速评估[J].装备环境工程,2014,11(6):148-152. ZHOU Kun,QIAN Han-bo,ZHOU Yi,WANG Cheng-zhang,WANG Jin-mei.Fast Evaluation of Storage Life of Missile Nonmetal Weak Links[J].Equipment Environmental Engineering,2014,11(6):148-152. |
导弹非金属薄弱环节贮存寿命快速评估 |
Fast Evaluation of Storage Life of Missile Nonmetal Weak Links |
投稿时间:2014-08-04 修订日期:2014-12-15 |
DOI:10. 7643 / issn. 1672-9242. 2014. 06. 025 |
中文关键词: 导弹 非金属薄弱环节 贮存寿命 快速评估 |
英文关键词:missile nonmetal weak link storage life fast evaluation |
基金项目: |
|
Author | Institution |
ZHOU Kun | No. 59 Research Institute of China Ordnance Industry, Chongqing 400039, China |
QIAN Han-bo | Coordination and Association Center of SASTIND, Beijing 100081, China |
ZHOU Yi | No. 59 Research Institute of China Ordnance Industry, Chongqing 400039, China |
WANG Cheng-zhang | No. 59 Research Institute of China Ordnance Industry, Chongqing 400039, China |
WANG Jin-mei | No. 59 Research Institute of China Ordnance Industry, Chongqing 400039, China |
|
摘要点击次数: |
全文下载次数: |
中文摘要: |
目的 科学评估某型导弹 4 类 80 种非金属薄弱环节的贮存寿命。 方法 建立由分析、试验、评估、验证等 4 个层次工作组成的贮存寿命快速评估流程。 以实验室加速老化试验、自然环境试验、对比试验、经验数据分析为手段,按照基于实验室加速老化试验结果定量评估、基于已有加速老化试验数据定量评估、基于对比加速老化试验结果半定量评估、基于近似产品经验数据定性评估等 4 种方法开展了试验评估工作。 结果 以天然橡胶 1161、JZ101-67 高阻尼减振器、天然橡胶 1157、特 221 润滑脂等 4 种非金属薄弱环节为 4 种方法应用示例,得出了 4 种非金属薄弱环节贮存寿命都大于 23 年的评估结果。 结论 4 种非金属薄弱环节多能满足延寿工程的要求。 |
英文摘要: |
Objective To scientifically evaluate the storage life of 4 types and 80 kinds of nonmetal weak links in a type of missile. Methods The fast evaluation process of storage life was built by four working levels, namely, analysis, test, evaluation, and verification. By means of laboratory accelerated aging tests, weathering tests, contrast tests and experience datum analysis, the storage life was evaluated using 4 method, including quantitative evaluation based on the laboratory accelerated aging tests, quantitative evaluation based on the existing accelerated aging tests data, semi-quantitative evaluation based on the contrast tests and qualitative evaluation based on the experience datum analysis. Results The natural rubber 1161, the JZ101-67 High damping shock absorber, the natural rubber 1157 and the 221 Grease were taken as the examples for application of the 4 methods. And the evaluation results showed that the storage life of all 4 types of nonmetal weak links was more than 23 years. Conclusion All the 4 types of nonmetal weak links met the requirements of life extension project. |