A Method of Increasing Airtight Function of Hard Chromium Plating |
Received:May 07, 2012 Revised:August 15, 2012 |
View Full Text View/Add Comment Download reader |
DOI: |
KeyWord:airtight function hard chromium plating sealing-treatment |
Author | Institution |
TANG Zhi-hui |
Beijing Institute of Aeronautical Materials, Beijing , China |
WANG Chang-liang |
Beijing Institute of Aeronautical Materials, Beijing , China |
WANG Li-qiang |
Chengdu Aircraft Industrial(Group)Co. Ltd., Chengdu , China |
DAI Shu-cheng |
Chengdu Aircraft Industrial(Group)Co. Ltd., Chengdu , China |
YUE Wen-hua |
Beijing Institute of Aeronautical Materials, Beijing , China |
LU Feng |
Beijing Institute of Aeronautical Materials, Beijing , China |
|
Hits: |
Download times: |
Abstract: |
The causes of poor airtight performance of hard chromium plaiting were analyzed. A sealing-treatment was employed in the post-treatment of hard chromium plaiting to improve the airtight function of the coating system. The results showed that the hard chromium plaiting passes 20 MPa/30 min airtight function testing with no leakage of gas after the post-treatment by 518 sealing reagent; the sealing reagent penetrates as deep as 20~30 μm and co-operates well with hydraulic fluid. |