Storage Life Prediction of Fluorine Rubber Products Based on Accelerated Aging and Natural Storage Data
Received:June 24, 2014  Revised:July 01, 2014
View Full Text  View/Add Comment  Download reader
DOI:10.7643/issn.1672-9242.2014.04.013
KeyWord:natural storage  accelerated aging  rubber sealing  storage life
        
AuthorInstitution
MA Tong-ling Beijing Power Machinery Institute, Beijing , China
DANG Xiao-yong Beijing Power Machinery Institute, Beijing , China
PANG Ming-lei The 53rd Institute of Weapon Equipment, Jinan , China
Hits:
Download times:
Abstract:
      Objective To accurately evaluate the storage life of fluorine rubber products. Methods The accelerated storage test data were verified using the natural storage data of fluorine rubber G402. Results The results confirmed the feasibility of the accelerated aging test method and the reliability of the data. The failure threshold was determined through the simulation test in accelerated aging test. Conclusions It was predicted that the storage life of fluorine rubber G402 products reached up to 15 years.