Analysis of the Spatial Variability of the Initial Corrosion Rate of Three Steel in the East China Sea
Received:July 13, 2021  Revised:August 07, 2021
View Full Text  View/Add Comment  Download reader
DOI:10.7643/issn.1672-9242.2021.10.011
KeyWord:East China Sea  corrosion  typical steel  geostatistical analysis  spatial variation characteristics
           
AuthorInstitution
MA Shao-zheng Key Laboratory of Marine Environmental Corrosion and Bio-fouling, Institute of Oceanology, Chinese Academy of Sciences, Qingdao , China;University of Chinese Academy of Sciences, Beijing , China;Open Studio for Marine Corrosion and Protection, Pilot National Laboratory for Marine Science and Technology, Qingdao , China
SUN Hu-yuan Key Laboratory of Marine Environmental Corrosion and Bio-fouling, Institute of Oceanology, Chinese Academy of Sciences, Qingdao , China;Open Studio for Marine Corrosion and Protection, Pilot National Laboratory for Marine Science and Technology, Qingdao , China
SUN Li-juan Key Laboratory of Marine Environmental Corrosion and Bio-fouling, Institute of Oceanology, Chinese Academy of Sciences, Qingdao , China;Open Studio for Marine Corrosion and Protection, Pilot National Laboratory for Marine Science and Technology, Qingdao , China
WANG Zhao Key Laboratory of Marine Environmental Corrosion and Bio-fouling, Institute of Oceanology, Chinese Academy of Sciences, Qingdao , China;University of Chinese Academy of Sciences, Beijing , China;Open Studio for Marine Corrosion and Protection, Pilot National Laboratory for Marine Science and Technology, Qingdao , China
Hits:
Download times:
Abstract:
      To study the initial corrosion rate of X80, EH36 and 45# steel at 42 stations in the East China Sea, in this paper, the initial corrosion rate of X80, 45# and EH36 steel measured in the East China Sea in September 2019 were obtained by the potential polarization curve method. The data was analyzed by geostatistics to explore the spatial distribution and variation characteristics of the initial corrosion rate of the three steels in the study area, and draw the initial corrosion rate prediction map. The spatial distribution characteristics of the initial corrosion rate of each type of steel are as follows:the spatial distribution of the initial corrosion rate of 45# steel is higher in the southwest and lower in the northeast; the spatial distribution of the initial corrosion rate of EH36 steel is higher in the northeast, lower in the southwest; while the spatial distribution of the initial corrosion rate of X80 steel is obviously lower in the seas close to the Yangtze River estuary, and higher in other seas. The distribution of the initial corrosion rate of the three steels presents different characteristics. At the same time, statistical analysis shows that the average initial corrosion rate of the three steels in the East China Sea is 0.42 mm/a for X80, 0.49 mm/a for 45#, and 0.17 mm/a for EH36. In addition, the spatial variability of the initial corrosion rate distribution of the three steels in the East China Sea is obvious, and the spatial autocorrelation is strong. The nugget values of X80, 45# and EH36 are 0.0148, 0.0044, and 0.0017, respectively, and the range is between 1000~2000 km.